You need to consider the design thickness requirements for the particular line, which includes the corrosion allowance too. Based on the requirement you may decide whether the pipe can be used.
 
Regards
 
J.N.Murthy 

On Wed, Jan 20, 2010 at 12:52 PM, Gulam kader <armvasi@gmail.com> wrote:
Dear all,
 
We received one 40" elbow (ASME 16.9) ASTM A 860 material having so much pitting on full external surface. Which standard we can refer for the acceptance criteria? 
 
 
I referred in ASTM A 860, its talks about only depth of surface discontinuity(5% of the nominal thickness),  there is no detail about the area of the pitting allowance.
 
Please help me on this issue. Very urgent
 
Regards,
 
Gulam Kader 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...