Friday, January 1, 2010

Re: [MW:3937] WQT pipe dimensions

Dear 6".

--- On Thu, 31/12/09, Sreejith.Nair <fizzyshadow@gmail.com> wrote:

From: Sreejith.Nair <fizzyshadow@gmail.com>
Subject: [MW:3936] WQT pipe dimensions
To: materials-welding@googlegroups.com
Date: Thursday, 31 December, 2009, 4:37 PM

Can anybody please tell me what is the minimum required dimensions of test piece for the qualification of welders in 6G as per API 1104   



--
- Sreejith Nair-

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...