1. Both RT and UT Combination will be best. For surface PT is mandatory. 2. UT we can use Shear wave(SW) for fusion zone, Volumetric can use Angle beam Longitudinal wave(LW) (Single crystal for higher beam distance and Twin for Near zone) 3. Always better to reconfirm with LW probe wherever SW indication, because shear wave redirect. 4. Using LW for fusion zone probably higer sensitivity (More than code requirment) Regards, S.Senthilkumar
--- On Sun, 30/8/09, Nilesh Pathare <patharenil@gmail.com> wrote:
From: Nilesh Pathare <patharenil@gmail.com> Subject: [MW:3079] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates To: materials-welding@googlegroups..com Date: Sunday, 30 August, 2009, 2:18 PM
Hi, If your specification permits for RT or UT you can carry out any of these test for 60 mm Thick S.S. For RT you may need cobalt 60 or High strength iridium 192. For Ultrasonic Testing you shall use the RTD Twin crystal longitudinal wave Angle probes. Regards, Nilesh Pathare. On Sun, Aug 30, 2009 at 10:35 AM, Stephen <stephenipr@gmail.com> wrote: I wanted to know which NDT to be carried out for 60 mm thick austenitic stainless steel plates welded using TIG welding
-- Best Regards, Nilesh Pathare
Love Cricket? Check out live scores, photos, video highlights and more. Click here --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-