[MW:3080] Re: Regarding the NDT to be carried out for 60 mm thick austenitic stainless steel plates

hi,
           you can go for high strength - 192, but dont go for cobalt 60 since we use for thickness ranging more than 100 to  & 150 mm above.

On Sun, Aug 30, 2009 at 11:48 AM, Nilesh Pathare <patharenil@gmail.com> wrote:
Hi,
If your specification permits for RT or UT you can carry out any of these test for 60 mm Thick S.S.
For RT you may need cobalt 60 or High strength iridium 192.
For Ultrasonic Testing you shall use the RTD Twin crystal longitudinal wave Angle probes.

Regards,
Nilesh Pathare.

On Sun, Aug 30, 2009 at 10:35 AM, Stephen <stephenipr@gmail.com> wrote:

I wanted to know which NDT to be carried out for 60 mm thick
austenitic stainless steel plates welded using TIG welding





--
Best Regards,

Nilesh Pathare




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...