[MW:3077] Re: PQR FOR A570Gr40 and A570 Gr36

both belongs to S#1 Gr#1 (refer QW 422 of ASME BPV Section IX)
yes, you can use since both belongs to same grouping

On Sun, Aug 30, 2009 at 9:46 AM, Samimi Mottagi, Alireza <Samimi@mapnagenerator.com> wrote:

HI

Kindly please inform me that I have two material  A570Gr40 and A570 Gr36 and I want to know where in Asme Standard I can find the P no. and Gr no. of them and according to Asme if I take a PQR on A 570 Gr 36 is it cover the A570 Gr 40 or not. Please give me the coorect address of standard.

thanks



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...