Friday, August 28, 2009

[MW:3063] Re: Distortion limit for ASME Section 8 Vessels

Dia of the Vessel- 2m
Shell, Head thickness-6mm
Design Pressure-Atmospheric pressure.
 
Regards
Prabhakar. S

On Fri, Aug 28, 2009 at 1:23 PM, Arunachalam A <arunvani@gmail.com> wrote:
Code ASME Section VIII Div 1 talks the following tolerances:
 
1. shell/head ovality. as per UG 80/81
2. Fit up tolerances as per UW33
3. Weld reinforcement tolerances as per UW 35.
 
You need to assess the acceptance of tank/vessel based on the above tolerances.
 
Please give the design parameters of the vessel ( shell dia/thick/internal pressure/external pressure  etc). in order to assess the vessel
 
arun


 
On Fri, Aug 28, 2009 at 11:12 AM, prabhakar s <prabhakars84@gmail.com> wrote:

Hi,

 

 

We have procured a Stainless Steel tank from one of our sub contrators. The thickness of the plate is 6mm. They have done hydrotest also. The tank is shifted to our Project site from the Sub contractors yard. We observed a distortion of 3mm near a Longitudinal seam (Both side of the weld seam).

 

I would like to know the allowable tolerance limit for distortion. Is 3mm acceptable? If it is so please give me the code reference.

 

We observed  a Grinding mark of 0.5 mm depth on 6mm thick Shell. what is the allowable limit for this? Is there any code reference?

 

Your early response in this regard will be highly appreciated.

 

 

Regards

Prabhakar. S

 






--
ARUNVANI

If you want help, help other,
If you want trust, trust others,
If you want Love, spread it away,
If you want friends, be a True one.

If you want a great TEAM, Be a Great TEAMMATE.

Teamwork is less "EGO" and more "We Go"

The great Companies and Teams are those,
That share the similarities,
and celebrate the differences.

They seek harmony, not uniformity.
They hire Talent, not Color or Caste.
They strive for oneness, not sameness.

No one goes alone to the height of Excellence.
Your Success will depend on others,
And theirs will depend on You.

Remember, the meaning of Team is
T : Together
E: Everyone
A: Achieves
M : More




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...