Friends ,
 
thanks for hte below guide line ,
 
Here i am looking for more details instead of knowing the whole volume of metal required .
 
I would lke to know the quantity for each type of electrode as we have for eg TIG root and hot pass followed with 7016 or
 
root is down hill and the other pasess are up hill ,
 
Do any one know how to find this or any Excel  program as most of the time need to depend of the supplier or welding formans .
 
Any helping hand will be appreciated .
 
Regards
 
Sujeet
On Wed, Aug 26, 2009 at 4:30 PM, daniel iordache <daniel.iordache@gmail.com> wrote:
Hi,

maybe that help you ....

in part ....

Regards

On Wed, Aug 26, 2009 at 8:12 AM,
chandergirotra@gmail.com<chandergirotra@gmail.com> wrote:
>
> REPLY
>
> Dear Member/s,
>
> THe quickest method is to fist  calculate volume of  the V- groove .
> Multiply this volume with density to get theoreticall weight of weld
> metal. Now we know that the actual weight used is much more than the
> theoretical weight since there are butt losses,electrode coating has
> to be accounted for and there is convexity at the top and  root of
> joint.
> Thus the  weld metal weight therefore =theoretical weight xQ factor
> ( Quantity  factor) .This Q factor=2 for TIG welding and 2.5 for SMAW.
>
> Hope this thumb rule will help you calculate weight of  welding
> electrode/wire required for a joint..
>
> Sorry that for your second query for gas consumption I am unable to
> respond.
>
> Chander Girotra
> ==========================================================================================================================
>
> On Aug 25, 2:48 pm, Sujeet Sangle <sujeetsan...@gmail.com> wrote:
>> Dear Memebers ,
>>
>> I need to calculate quantity for SMAW consumable  for Structural Electrodes
>> for V Groove different thickness and Diameter
>>
>> TIG consumable for piping work different thickness and Diameter .
>>
>> Together with the Pre heating gas consumption .
>>
>> Can any one guide me for the above .
>>
>> Thanks
>>
>> Sujeet
>
> >
>



--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...