Friday, August 28, 2009

[MW:3053] RE: 3048] Re: Record of RT

Please let me know more about this (Thio-sulphate Technique ) and other techniques used.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vipin george
Sent: Friday, August 28, 2009 11:54 AM
To: materials-welding@googlegroups.com
Subject: [MW:3048] Re: Record of RT

 

Hi!

The conventional way to keep record is to use a Thio-sulphate Technique.

 

Rgds,

Vipin

On Wed, Aug 26, 2009 at 9:34 AM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:

Dear all,

Is there any facility to keep records of radography films ( including radiographic view ) on  pc,so that even if RT films get damaged, we could have permanant records of the same.

Tanx & Rgds.

psp

 


See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz<br


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...