as little as possible, always weld from the centre outwards in a 'stitch welding' progression
 
 
Nick Davies
 
  

On Wed, Aug 26, 2009 at 7:29 PM, bdsathiyamoorthy <bdsathiyamoorthy@gmail.com> wrote:

Dear All,
Pls any one can suggest to me that  We are using API 650 (Year 2005)
tank fabrication, Now the problem bottom plate distration tolerance
not able to get from  API 650. Kindly I request to all  please any one
can suggest to me what is the tolerance of bottom plate distration.

Thanks in advance,


--
Regards,

Nick Davies

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...