Monday, August 24, 2009

[MW:3003] Re: Fw: [MW:2985] A350 Gr P22 purging

Dear k zamani,
A 350 Gr P22 is not listed/stated in ASME IX..may be you meant a A335 Gr P22 (2.25Cr–1Mo). Based on API 582 back purging is required for the GTAW and GMAW processes for welding materials having a nominal chromium content greater than 2 1/4% unless the joint is ground or back gouged to sound metal
Tong2je


On Sat, Aug 22, 2009 at 5:56 PM, Ahmed Osman <a.osman81@yahoo.ca> wrote:
there is nothing A 350 Gr P22 but " A 335 " Gr P22 and it dose not need pack purging

Best Regards ,
ENG. Ahmed Osman
TEL. +213 793092233


--- On Sat, 8/22/09, kambiz zamani <kambiz_zamani50@yahoo.com> wrote:

From: kambiz zamani <kambiz_zamani50@yahoo.com>
Subject: [MW:2985] A350 Gr P22 purging
To: materials-welding@googlegroups.com
Received: Saturday, August 22, 2009, 7:12 AM

Dear All , i want to know that A350 Gr P22 required to argon back purging (GTAW process) or not?                           regards ,k zamani IRICO. cswip3.1 welding inspector



Ask a question on any topic and get answers from real people. Go to Yahoo! Answers.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...