[MW:3002] RE: 2997] RE: 2996] Technical Query on ASME Sec-IX ( QW-403.5)

Yes

All mentioned joints you can weld with the same WPS if we don’t change any essential & sup-Essential variables.  

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Monday, August 24, 2009 8:29 AM
To: materials-welding@googlegroups.com
Subject: [MW:2997] RE: 2996] Technical Query on ASME Sec-IX ( QW-403.5)

 

No,

It applies to different group number within same P number, and not with different P numbers.

Any way why you are impact testing this combination (P1 # P8), what are your design conditions?

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sukamal Naskar
Sent: Monday, August 24, 2009 9:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:2996] Technical Query on ASME Sec-IX ( QW-403.5)

 

Dear All,

Good Morning !!!

 

I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )

 

QW-403.5 (c ) , states that “ ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified.”

 

Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1 material using  SMAW ( E 309MoL) process with impact testing  on weld metal & both HAZ portion , does this PQR supports the following WPS combination of base metals , if all other welding variables are unchanged ?

 

(i)                  P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2 

(ii)                P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1 

(iii)               P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1 

 

Please give your comments,

 

Thanking you,

Regards,
--
Sukamal Naskar
Malaysia

 


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...