Best way is to qualify the PQR on Butt Joint as per sec IX and this will allow you to weld fillet of any size
Regards
Hegde
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Endri Prasetyo
Sent: Saturday, August 01, 2009 10:43 AM
To: materials-welding@googlegroups.com
Subject: [MW:2855] WPS/PQR for fillet weld
Dear Experts,
I have a joint as shown in the attachement. It is a fillet joint, GMAW process, 2FR position.
Please advise me how can I make a test spesimen to establish a WPS and PQR based on AWS D1.1.?
Thanks in advance.
Regards,
Endri
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments