Mr Kataiah, Is something not correct here? Shashank Vagal
--- On Mon, 29/6/09, kataiah@bilfal.com <kataiah@bilfal.com> wrote:
From: kataiah@bilfal.com <kataiah@bilfal.com> Subject: [MW:2569] Fw: [MW:2566] Re: lifetime of a qualified WPS To: "Materials & Welding" <materials-welding@googlegroups.com> Date: Monday, 29 June, 2009, 10:33 AM
Dear Mr.Raghuram If code changes after some years & there is a change in essential/supplementary essential variables, the wps will be valid. regards P.Kataiah ----- Forwarded by Kataiah/BelleliSA on 29/06/2009 07:44 ص -----
| "BR" <raghurambathula@gmail.com> Sent by: materials-welding@googlegroups.com 29/06/2009 07:37 ص Please respond to materials-welding | To: "Materials & Welding" <materials-welding@googlegroups.com> cc: Subject: [MW:2566] Re: lifetime of a qualified WPS | None, yes its forever as long as it represents your production weld. However changes may be made in the nonessential variables of a WPS to suit production requirements without requalification provided such changes are documented with respect to the essential, nonessential, and, when required, supplementary essential variables for each process. This may be by amendment to the WPS or by use of a new WPS. Changes in essential or supplementary essential (when required) variables require requalification of the WPS (new or additional PQRs to support the change in essential or supplementary essential variables). On Jun 29, 8:28 am, sandy kumar <sandy001...@gmail.com> wrote: > Can anyone tell whats is the validity period of a qualified WPS?
|
Looking for local information? Find it on
Yahoo! Local --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
No comments:
Post a Comment