Try F series ASTM standards like ASTM F467 and 468
On Fri, Jul 3, 2009 at 9:30 AM, Agrawal Sunil (Mumbai -Stequ) <S.Agrawal@ticb.com> wrote:
Can anyone let me know the ASME material designation for the material specified by our client "SF 468 UNS R50400 TI Gr 2" for Ti bolts. I am not able to get this material in ASME Sec II Part B.
Best Regards,
Sunil Agrawal
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---