[MW:2614] Re: quality of water to be use for SS piping hydrotest

Hi,
 
Please refer Note given in clause 5.7 of API 570  for this clarification
 
Regards,
 
K.Babu
 
Singapore


 
On Thu, Jul 2, 2009 at 10:46 AM, Dilip Kumar <dilipkumar@ctci.co.th> wrote:

Dear friends,

 

I would like to have your opinion about the subject, and if any one have supporting document in the form of code and practices, previously done or various company method statement's to support the potable water to be use for hydrostatic testing for SS piping.

 

Thanks

 

With regards.

 

dk

 

 







--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...