Tuesday, May 12, 2009

[MW:2155] RE: 2154] Recertification of old consumables

No – Not good welding practice

 

John du Plessis

Technology Manager

Southern African Institute of Welding

+27 11 2982103 (T)

+27 11 8364132 (F)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kataiah@bilfal.com
Sent: 12 May 2009 06:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:2154] Recertification of old consumables

 


Dear Friends,

Shall i use old consumables (10 Years old) to currents jobs (as per ASME 2007) without  any recertification.
if yes, Pl. provide code reference.

regards
P.K
K.S.A
0096543637487 <br


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...