Thursday, May 7, 2009

[MW:2117] Re: preheat SA- 516 gr 70


It depends on thickness.
What is the thickness?

Thanks & Regards
----------------------------
Narendra Gohil
Welding Engineer
QAFCO
Ph.00974-4228289(O)
Mo.00974-6044289
Email: ngohil@qafco.com.qa

P Save a tree.  

Please don't print this e-mail unless it's really necessary.



From: "SAUL VASQUEZ T." <svasquez@ingetanques.com>
To: <materials-welding@googlegroups.com>
Date: 07/05/2009 04:50
Subject: [MW:2114] preheat  SA- 516 gr 70
Sent by: materials-welding@googlegroups.com





 
Dear   all
 
We are   API 650 steel tanks with  steel ASTM  516 gr70 and our client requests that preheat to 70°C - 100°C is this correct? The API 650   code section 7-1 that says that  preheat at 10°C


thanks all

 
 
 
Cordial saludo
Kind regards
Saul Vasquez T.
--------------------------------
INGETANQUES LTDA
Cra 8B Nº 190-81 
Tel. 57 (1) 6794382  Fax 57 (1) 6723793
CEL. 320-3469363  y  316-5388051
Bogota D.C.    Colombia.  http://www.ingetanques.com/
 
P Antes de imprimir este mensaje, asegúrese que es necesario. El medio
ambiente está en nuestras manos. No malgastes los recursos. Ten en cuenta
que son limitados.

 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...