hi
i will run a repair welding qualification according to DNV F101(one for throught thickness,one for partial thickness)..now contractor requist that two qualification are done in a one test sample in different location.
how specify locations for sampling ?(in this standard it's a figure for sampling in appendix c for qualification original weld, that attached )
if anybody have detailed information,i will be grateful for sharing it.








--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...