Pressure rating of any flange is depends on its thickness, PCD of Holes and number of holes and gasket type and design.
Regards
paresh
On Sat, May 2, 2009 at 8:44 AM, Ali Asghari <asghariali@rocketmail.com> wrote:
hican anybody explain .how is it possible that a product such as flange made from a given material can have different pressure classes?if the fabrication process is also same ,how?regard advanc
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
No comments: