Monday, March 30, 2009

[MW:1840] RE: 1838] Fabricated Stiffeners

Dear Devang,

Fabricated stiffeners can be used in external pressure design of shell
of
pressure vessel as per ASME Sec. VIII Div.1. You can refer UG -29 , Fig.
UG 29.1 , UG-30 & Fig. UG-30 of ASME Sec. VIII Div.1 for more details on
the acceptable method of attaching stiffener rings

Regards

Somesh Kumar Pandey
KBR Energy & Chemicals
79 Anson Road #20-01
Singapore 079906
Office: +65 6210 7459
Fax: +65 6210 7250
Email: Somesh.Kumar@kbr.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Devang Patel
Sent: March 30, 2009 12:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:1838] Fabricated Stiffeners


can we use fabricated stiffeners in external pressure design of shell of

pressure vessel?

If, yes than please tell, can we use staggered intermittent weld to
fabricate T or Angle?

Please reply.


Regards,


Devang Patel
Manager Engineering

INOX INDIA Ltd.
Ph :+91-265-3056392-3056100
Fax :+91-265-2333398-2341449
email : devangp@inoxindia.com
www.inoxindia.com

This e-mail, including any attached files, may contain confidential and privileged information for the sole use of the intended recipient. Any review, use, distribution, or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive information for the intended recipient), please contact the sender by reply e-mail and delete all copies of this message.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...