Tuesday, March 17, 2009

[MW:1774] Socket welding gap

We're welding Socket-welding fittings from 3/8 to 2", and we have
trouble with the internal offset requested on ASME B31.3.

Our client hasn't accepted the usual method, which consist in use a
"elastic welding spacer" (US patents related: 4,505,420 or 4,346,918
or Google: gap-a-let).

Is there another method, e.g.: an external device - that can be used
for this welding, ensuring the correct gap [1.6 mm] ?

I know that's a materials related forum, but I'm sure you guys can
help me.

Regards.
Salvador.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...