[MW:1766] RE: 1732] Re: Tolerance of flange joint

You may refer PFI standard ES3

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
pjoshi@technip.com
Sent: Saturday, March 07, 2009 6:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:1732] Re: Tolerance of flange joint

It depends on the Flange standard you are following. For e.g. refer ASME
B16.5, para 7.8 for tolerance on the mismatch of the drilled holes/BCD.
For
other standards, you may have to refer to the appropriate standards,
referred therein.

Best regards,

Prasad


mick nest

<crc1199@hotmail.

com>
To
Sent by:
<materials-welding@googlegroups.com
materials-welding >

@googlegroups.com
cc


Subject
07/03/09 07:11 AM [MW:1714] Tolerance of flange
joint

Please respond to

materials-welding

@googlegroups.com

Dear All.

Please let me know what is the tolerance ( misalignment ) for two
flanges
joint together by stud bolts as per any standard.

Regards,

Mick


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...