Monday, March 16, 2009

[MW:1765] RE: 1764] Hot Induction Bend

Hi VJV,
Cold cutting is always preferable than hot or gas cutting, as cold
cutting will not alter metallurgical properties.
One of other things to be considered is profile to suit the ID/OD of the
joining pipe/fitting.

Ravi

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of VJ V
Sent: Sunday, March 15, 2009 5:30 PM
To: Materials & Welding
Subject: [MW:1764] Hot Induction Bend


Hi All,

Is there any technical adversity in Cold cutting a Hot induction Bend
( Hot formed at around 860 Deg C and then Stress relieved) to suite to
site condition ? I think Hot work-oxy aceteline cutting etc- is not
acceptable...

But Can the Hot Induction Bend be undergone cold cutting...
other than Metallurgical consequence any thing else to be considered
while cold cutting ?

Thanks
VJV


~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

This email message is for the sole use of the intended
recipient(s) and may contain confidential and privileged
information of Cameron and its Operating Divisions.
Any unauthorized use or disclosure is prohibited.
If you are not the intended recipient, please contact the
sender by reply email and delete and destroy all copies
of the original message inclusive of any attachments.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...