Sunday, March 15, 2009

[MW:1764] Hot Induction Bend

Hi All,

Is there any technical adversity in Cold cutting a Hot induction Bend
( Hot formed at around 860 Deg C and then Stress relieved) to suite to
site condition ? I think Hot work-oxy aceteline cutting etc- is not
acceptable...

But Can the Hot Induction Bend be undergone cold cutting...
other than Metallurgical consequence any thing else to be considered
while cold cutting ?

Thanks
VJV

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...