Skip to main content

[MW:1005] Re: 1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503 -224 -GR. 28

OKAY. THANKS FOR YOUR INFORMATION.

REGARDS,

S.N.DAVE

--- On Thu, 8/7/08, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

> From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
> Subject: [MW:1004] RE: 1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503 -224 -GR. 28
> To: materials-welding@googlegroups.com
> Date: Thursday, August 7, 2008, 3:32 PM
> Why don't you check in EN 10222 for the required grade?
> As BS 1503 is
> obsolete, no use of searching for similar of equivalent
> grades.
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> shailesh dave
> Sent: Thursday, August 07, 2008 3:26 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE
> OF BS1503
> -224 -GR. 28
>
>
> YES IT IS FORGING MATERIAL.
>
> REGARDS,
>
> S.N.DAVE
>
>
> --- On Thu, 8/7/08, Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com> wrote:
>
> > From: Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com>
> > Subject: [MW:1000] RE: 999] Re: 993] EQUVIVALENT ASME
> GRADE OF BS1503
> -224 - GR. 28
> > To: materials-welding@googlegroups.com
> > Date: Thursday, August 7, 2008, 3:22 PM
> > Is it a forging material? BS1503 is superseded and
> replaced
> > by EN 10222,
> > please check?
> >
> > ________________________________
> >
> > From: materials-welding@googlegroups.com
> > [mailto:materials-welding@googlegroups.com] On Behalf
> Of
> > shailesh dave
> > Sent: Thursday, August 07, 2008 2:28 PM
> > To: materials-welding@googlegroups.com
> > Subject: [MW:999] Re: 993] EQUVIVALENT ASME GRADE OF
> BS1503
> > -224 - GR.
> > 28
> >
> >
> >
> > Dear Mr. Rohit,
> >
> >
> >
> > Thanks for the information. I have gone through it but
> it
> > does not say
> > specifically about224 - GR. 28
> >
> >
> > Would you pl. thorw some more light on this.
> >
> >
> >
> > Regards,
> >
> >
> >
> > S.N.Dave
> >
> > --- On Tue, 8/5/08, Rohit Bafna
> <rohit@tcreng.com>
> > wrote:
> >
> > From: Rohit Bafna <rohit@tcreng.com>
> > Subject: [MW:994] RE: 993] EQUVIVALENT ASME GRADE OF
> > BS1503 -224
> > - GR. 28
> > To: materials-welding@googlegroups.com
> > Date: Tuesday, August 5, 2008, 9:05 PM
> >
> > Dear Mr. Dave,
> >
> > Please look at
> http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm
> > <http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm>
> >
> > Regards,
> >
> > Rohit Bafna
> >
> > Director - Global Sales
> >
> >
> >
> > From: materials-welding@googlegroups.com
> > [mailto:materials-welding@googlegroups.com] On Behalf
> Of
> > shailesh dave
> > Sent: Tuesday, August 05, 2008 8:39 AM
> > To: materials-welding@googlegroups.com
> > Subject: [MW:993] EQUVIVALENT ASME GRADE OF BS1503
> -224 -
> > GR. 28
> >
> >
> >
> > DEAR MEMBERS,
> >
> > CAN ANYBODY LET ME KNOW THE EQUIVALENT ASME GRADE OF
> > BS1503 -224-GR.28.
> > WHERE FROM I CAN HAVE THIS INFORMATION AS READY
> RECKONER.
> >
> > REGARDS,
> >
> > SHAILEH
> >
> > QA/QC INCHARGE
> >
> > ADGAS DAS ISLAND UAE
> >
> >
> >
> >
> >
> >
> >
> >
> >
> >
>
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...