[MW:1016] [piping_valves] extended bonnet valves for high temperature service


Though such high temp valves do exist, but few in the plants and are specialized construction, due to the temp/press and service and the location of the valve and safety requirements.

The extended bonnet construction is one option to dissipate heat and to lower the heat at the stem packing similar to the reduction of cryogenic valve temp propagation to the stem packing and to avoid subsequent failure of the packing and operation of the valve. In all, the subject of concern is the stem packing failure. Other options are finned bonnet constr, stem packing with separate cooling system.

Protection for valve handwheel operation is not a major concern as it can be chosen as Motor/Pneumatic operated valve. Most of the hand operated valves requires once in a year operation in such high temp service.

Coming to the stem packing,
1)The usual ones are in one or more combination of graphite, metal rings, Elastomer rings, Lip seals, simple TEFLON rings etc.
2) In the moderately higher temp. range, only Graphite+alloy is used in diff. arrangements.
3) For very high temp such as your case, cooling system or the extended bonnets and same as 2) packings are used. Also many new proprietary packing arrangements are available in the market. Evaluating them is an important part of a material engineer's role.

Additional one to be noted is, the valve basic design is also to be reviewed. Process engr. is not a valve specialist. So the material engineer is supposed to evaluate such cases. In this case a rising stem valve type design to be avoided as it has vertical and rotation wearing on the packing. For controlling a butterfly valve could be evaluated. For Gate types, a knife gate valve could be thought of. Pl. take note that  such evaluation has many things to be accounted for such as leakage allowance, emission, hazops, ATEX concerns, operation difficulty, trim erosion and not the least process parameters like pressure drops, zigma allowance, opening/closing period, service fluid etc.

Coming to your question,
1) Parameters controlling the bonnet height ...depends on the stem packing design and heat propagation to the packing. As a thumb rule for alloy constr. 250mm shall be the min. height.
2) On tests....apart from the usual tests, service condition test is required to be performed. But if the manufacturer has a prototype test certificate, it could be accepted. Again it depends on the application of the valve. In your case prototype should be OK, in my opinion.
3) Create these valves as special parts and specify the individual condition of operation and design to ensure correct valve/packing design is offered by manuf.

*****
Important note is the temp you specified and the valve material specified does not go well together. Being a HP steam and at 700 deg. c(which itself is very unusual), SS is no good and it has to high alloy grade. Or your design condition is to be verified. B16.34 defined the temp. limits in the notes of every rating table.
*****

Regards,
Kannan.



"Herur Satyanarayana Shyam \(External\)" <SatyanarayanaShyam.Herur.Guest@snamprogetti.eni.it>
Sent by: piping_valves@yahoogroups.com

11/08/2008 10:03

Please respond to
piping_valves@yahoogroups.com

To
<materials-welding@googlegroups.com>
cc
<piping_valves@yahoogroups.com>
Subject
[piping_valves] extended bonnet valves for high temperature service





Dear friends

I have a query related to valves used at very high temperature for the refinery in Russia Im working on. The service are high temperature hydrocarbon, process with hydrogen or hot air and high pressure steam with ratings of 300# and 2500#. Design temperatures(stream list not yet issued by process) in FEED contractor piping class are 700 to 750 degC. Valve material(CF8, C>0.04)The FEED contactor has put a note against the valves(gate and globe) in his pipng class ' valves shall be supplied with extended bonnet and heat dissipating elements to obtain a packing temperature of 450degC maximum'. We have come across extended bonnet valves for cryogenic service.I would like to know if members have experience with extended bonnet valves for high temperature service. What are the parametres to be considered by the vendor in deciding the height of the bonnet? What are the tests/set up to be performed by the vendor to demonstrate that temperature at packing is <450°C.Is it feasible to have a extroordinarily long bonnet  in order to maintain T<=450 deg C?? What are the other packing materials other than graphite that can be used to compensate for the height of the bonnet. line gaskets are spiral wound with SS304H windings and mica/graphite filler.
 
Regards
Shyam --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

diverter valve said…
nice post. ived been searching for articles about valves and actuators and your post really helps. thanks a lot for posting this.

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...