Dear Dave,
PMI can tell you the % of the contains like Ni, mo etc. Based on this % we can check our requirement.
 
Regards,
 
Jani Pinakin



----- Original Message ----
From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
To: materials-welding@googlegroups.com
Sent: Monday, 24 March, 2008 2:42:02 PM
Subject: [MW:686] PMI TESTING OF SS 304L

Probably spectro isort by Amtek can detect C, (thou I have not used it), you can try at www.spectro.com

 

Also Arcmet930 by Metorex can detect C

 


From: shailesh dave [mailto: snd2988@yahoo.com ]
Sent: Monday, March 24, 2008 2:07 PM
To: materials-welding@googlegroups.com
Subject: PMI TESTING OF SS 304L

 

DEAR MEMBERS,

 

CAN ANYBODY TELL ME WHAT TECHNIQUE SHOULD BE USE TO PERFORM PMI OF SS304L. SINCE CARBON ANALYSIS IS VERY VERY IMPORTANT.

 

REGARDS,

 

S.N.DAVE

 

QA/QC MANAGER - TATA PROJECTS,

 

IWPP -III, SHUIBAH , SAUDI ARABIA






Get the freedom to save as many mails as you wish. Click here to know how.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...