Tuesday, March 25, 2008

[MW:693] Re: 683] Re: Section IX QW 200.4(b)

Is it 20 or 200? It might be 200..

On Mon, Mar 24, 2008 at 7:04 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

You can use combination of these processes to weld a base metal thickness (T) of up to 20mm max.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shabbir ahmad
Sent: Saturday, March 22, 2008 2:07 PM
To: materials-welding@googlegroups.com
Subject: [MW:683] Re: Section IX QW 200.4(b)

 


Yes Sanjeev

 

U can use GTAW for root deposit as per QW 200.4b.

 

shabbir
 

On 3/21/08, jitendra Thakor <jitendrathakor@gmail.com> wrote:


Dear Sanjeev

As per QW200.4(b) it is mandatory that your GTAW PQR thickness should
be minimum 13 mm. than you use GTAW as root as qualified in PQR.

Regards
Jitendra

On Fri, Mar 21, 2008 at 2:11 PM, sajeev c.g <sajeevmech@yahoo.com> wrote:
> Dear all,
>
> I have to prepare a WPS from two PQR's as per section IX.
> PQR 1 qualified in 10mm coupon full GTAW
> PQR 2 qualified in 40mm coupon SMAW+SAW(20mm deposit each)
>
> Can i write a WPS to weld GTAW (root) + SMAW+SAW?
> As per QW200.4(b) is it mandatory that the PQR 1 will be qualified in 13mm
> minimum to write a WPS as above?
>
> Regards
> sajeev
>
>  ________________________________
>
> Looking for last minute shopping deals? Find them fast with Yahoo! Search.
> >
>
<br





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...