Why not? Infact only sprak emission method can detect C, as these are not portables instruments maneuvering at construction sites is very difficult

Both Arc met and PMI Master (see the other post by Mr Nadig, WAS is from oxford instruments, US) are gas based, where the principle of Spectro isort is quite different, it neither use Argon nor X-ray source.

 

However take care while using spark emission on lighter wall components

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shailesh dave
Sent: Monday, March 24, 2008 2:58 PM
To: materials-welding@googlegroups.com
Subject: [MW:688] Re: PMI TESTING OF SS 304L

 

DEAR Mr. RAGHURAM,

 

THANKS FOR THE REPLY. JUST ADVISE ME IS IT RECOMMANDED TO USE SPARK EMISSION TECHNIQUE ON SS 304L MATERAIL FOR PMI.

 

AWAITING YOUR REPLY.

 

REGARDS,

 

S.N.DAVE

"Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com> wrote:

Probably spectro isort by Amtek can detect C, (thou I have not used it), you can try at www.spectro.com

 

Also Arcmet930 by Metorex can detect C

 


From: shailesh dave [mailto:snd2988@yahoo.com]
Sent: Monday, March 24, 2008 2:07 PM
To: materials-welding@googlegroups.com
Subject: PMI TESTING OF SS 304L

 

DEAR MEMBERS,

 

CAN ANYBODY TELL ME WHAT TECHNIQUE SHOULD BE USE TO PERFORM PMI OF SS304L. SINCE CARBON ANALYSIS IS VERY VERY IMPORTANT.

 

REGARDS,

 

S.N.DAVE

 

QA/QC MANAGER - TATA PROJECTS,

 

IWPP -III, SHUIBAH, SAUDI ARABIA


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...