[MW:688] Re: PMI TESTING OF SS 304L

DEAR Mr. RAGHURAM,
 
THANKS FOR THE REPLY. JUST ADVISE ME IS IT RECOMMANDED TO USE SPARK EMISSION TECHNIQUE ON SS 304L MATERAIL FOR PMI.
 
AWAITING YOUR REPLY.
 
REGARDS,
 
S.N.DAVE

"Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com> wrote:
Probably spectro isort by Amtek can detect C, (thou I have not used it), you can try at www.spectro.com
 
Also Arcmet930 by Metorex can detect C
 

From: shailesh dave [mailto:snd2988@yahoo.com]
Sent: Monday, March 24, 2008 2:07 PM
To: materials-welding@googlegroups.com
Subject: PMI TESTING OF SS 304L
 
DEAR MEMBERS,
 
CAN ANYBODY TELL ME WHAT TECHNIQUE SHOULD BE USE TO PERFORM PMI OF SS304L. SINCE CARBON ANALYSIS IS VERY VERY IMPORTANT.
 
REGARDS,
 
S.N.DAVE
 
QA/QC MANAGER - TATA PROJECTS,
 
IWPP -III, SHUIBAH, SAUDI ARABIA


Be a better friend, newshound, and know-it-all with Yahoo! Mobile. Try it now. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...