[MW:687] Re: PMI TESTING OF SS 304L

We are using PMI- Master Plus  supplied by WAS World wide Analytical System AG,Germany for PMI where carbon detection is needed.

Regards
Nadig


On Mon, 24 Mar 2008 Bathula Raghuram(Mumbai - PIPING) wrote :
>Probably spectro isort by Amtek can detect C, (thou I have not used it),
>you can try at www.spectro.com <http://www.spectro.com/>
>
>
>
>Also Arcmet930 by Metorex can detect C
>
>
>
>________________________________
>
> From: shailesh dave [mailto:snd2988@yahoo.com]
>Sent: Monday, March 24, 2008 2:07 PM
>To: materials-welding@googlegroups.com
>Subject: PMI TESTING OF SS 304L
>
>
>
>DEAR MEMBERS,
>
>
>
>CAN ANYBODY TELL ME WHAT TECHNIQUE SHOULD BE USE TO PERFORM PMI OF
>SS304L. SINCE CARBON ANALYSIS IS VERY VERY IMPORTANT.
>
>
>
>REGARDS,
>
>
>
>S.N.DAVE
>
>
>
>QA/QC MANAGER - TATA PROJECTS,
>
>
>
>IWPP -III, SHUIBAH, SAUDI ARABIA
>
>
>>



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...

ICL

Pages

Contributors

Blog Archive