[MW:675] Re: 664] Chemical cleaning for Marine boilers

Thanks for the information below. 
 
The chemical cleaning is for newly built boiler at yard and will be erected in FPSO.
We are doing chemical cleaning to remove mild scale and grease.
 
 
Thanks
Sriram.
 
On 3/19/08, donboscomarine@vsnl.net <donboscomarine@vsnl.net> wrote:

Dear Mr. Sriram,
You may please consult either Drew Ameroid or Unitor chemicals which are the standrad suppliers for chemicals in most of the ports. Here I am assuming, you are talking about a boiler fitted presently on the ship and not removed to the yard, as such. If at all the boiler is an exhaust gas economiser ( or exhaust boiler in Marine engineering terms) and is choked near the side where exhaust gas enters the shell, it is going to be extremely dificult and impossible at times to get the tubes cleaned internally by chemical circulation or soaking . If it is a new boiler then only a detergent plus mild alkali/ acid circulated and later a neutralising solution with fresh water washing will be enough.

Rgds.

G. A. Soman
Don Bosco Maritime Academy, Mumbai

----- Original Message -----
From: "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com>
Date: Wednesday, March 19, 2008 3:01 pm
Subject: [MW:665] RE: 664] Chemical cleaning for Marine boilers
To: materials-welding@googlegroups.com

> Is it new equipment or used one? What is the purpose of chemical
> cleaning for your equipment? (I mean incase of used equipment what
> typeof scaling involved, like water scales, iron oxide, and any other
> corrosion product/loose oxides?)
>
>
>
> The principle of cleaning basically consists of circulating the
> desiredchemicals through the Cooling Water Circuit by dosing them
> in the
> chemical dosing pot and maintaining circulation for a period
> sufficientto remove all the deposits.
>
>
>
> Sriram!
>
> Did u remember what we have done in BPB offshore for heat exchangers?
> What ever I could recollect I am putting down hereunder!
>
>
>
> The procedure is elaborated as follows:-
>
>
> CLEANING OF SHELL SIDE
>
>
>
>
> 1)                  Dosing of 2% Teepol B-300 into the Chemical Dosing
> Pot though which it is fed into the system.
>
>
>
> 2)                  The solution is circulated in the system for a
> period of 3-4 days during which KMnO4 value is tested.
>
>
>
> 3)                  On the completion of 4 days of circulation the
> system is to be progressively drained with simultaneous filling of
> freshwater.
>
>
>
>
> CLEANING OF TUBE SIDE
>
>
>
>
> This cleaning has been carried out by forming a closed circuit
> cleaningloop consisting of temporary piping and Recirculation Tank.
>
>
>
> 1)                  Filled and flushed the entire system with fresh
> water till clear.
>
>
>
> 2)                  2% Teepol B-300 and 0.5% KOH added based on the
> system volume into the circulation tank. This solution is then pumped
> into the exchanger where it is allowed to soak for a period of 12 hrs.
>
>
>
> 3)                  The same solution is then circulated for a
> period of
> 8 hrs, after which it is drained and flushed till the PH is equal to
> that of the flushing water.
>
>
>
> You can get the elaborated procedure from the chemical cleaning
> vendor,but remember it will vary for type of sediments what u
> needs to clean
> finally.
>
>
>
>
>
> ________________________________
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of jagannathan
> Sriram
> Sent: Wednesday, March 19, 2008 10:29 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:664] Chemical cleaning for Marine boilers
>
>
>
>
> Hi friends
>
>
>
> If any one has procedure for chemical cleaning of marine boilers
> pleaseforward to me.
>
>
>
> Thanks
>
> Sriram.
>
>
>
>
> >
>
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...