Re: [MW:10096] THROUGH THICKNESS DUCTILE TESTING

This test gives info about the resistance of plate to lamellar tearing. (Property reqd is %RA)
For more details on type of specimen and acceptance criteria please follow SA 770.
Regards,
Ravi

On Wed, Mar 2, 2011 at 1:45 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear members,
 
One of my client technical specification calls for through thickness ductile testing for plate thickness above 40 mm.
 
Can you give information about through thickness ductile testing & why we need to carry out this testing?
 
With kind regards.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...