Re: [MW:4015] Re: WELDING CONSUMABLE FOR SMAW & SAW

Or pipeliner from Lincoln Electric


From: Garry Hunt <garryhunt8@msn.com>
To: materials-welding@googlegroups.com
Sent: Fri, January 8, 2010 8:46:34 PM
Subject: RE: [MW:4001] Re: WELDING CONSUMABLE FOR SMAW & SAW

Have a look at the attached file from Bohler Welding
 
> Date: Fri, 8 Jan 2010 02:16:28 -0800
> Subject: [MW:3998] Re: WELDING CONSUMABLE FOR SMAW & SAW
> From: vanchinaths@gmail.com
> To: materials-welding@googlegroups.com
>
> PWHT for API pipe qualification will be as per ASME B31.3. Upto 19mm
> thickness PWHT is not required.
>
> On Jan 7, 2:52 pm, John Manoj <manojac...@gmail.com> wrote:
> > Dear all,
> >
> > I have to weld API 5L X70 to API 5L X70 butt joint.
> >
> > Can you help me to select welding consumable for SMAW & SAW process.
> >
> > I have selected 2 type of consumables i.e. Electrode E 9018G and Flux/Wire
> > F9AO-EA2-A3 or  Electrode E8018C3 and Flux/wire F8A2 -  EA2-A2.
> >
> > Which one is better? Is there any other proper electrode & flu/wire?
> >
> > and i wanted to know whether PWHT is applicable if we weld with these
> > electrodes.
> >
> > This is first time i am using this material.
> >
> > Your response is highly appreciated.
> >
> > Thanks
> > Manoj John.


Spread the cheer with Messenger for mobile. Learn more. --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...