PSL is "Product Specification Level".In case of PSL-1 impact testing is not mandatory and in case of PSL2 impact testing at 0 deg C is mandatory.There is a difference in Chemical composition requirements between PSL1 and PSL2.In case of PSL1 Yield Stress and UTS demands "min" value whereas in case of PSL2 there is a range of "min" and "max" for YS and UTS.
Regards

On Mon, Jan 4, 2010 at 7:51 PM, prakash kamathuru <prakashkbp@gmail.com> wrote:
Dear All,
 
Can Any one Explain me what is the difference between API 5L PSL-1 and PSL-2.What is the signefecance and where we need to use the specific PSL.
 
Regards,
 
Prakash K B

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...