Following is example to explain the conditions

 Condition 1

As per manufacturer (Say manufacturer ABC) the Flux and Wire combination mentioned on the data sheet and bag of flux is F7A8-EH12K and is inline with the ASME Sec II Part C SFA 5.17

Where "A" is as welded condition

PQR was qualified with PWHT using above mentioned manufacturers flux wire combination.

Question

1.       Can I write on my PQR and WPS write the Flux wire classification as F7P8-EH12K - NO FLUX-WIRE combination welding consumables shall be Qualified by Welding consumable Manufacturer. See below portions of ASME Sec.IIC.

Inline image
Inline image

2.       Batch of flux and wire used in PQR shall only be used in Production welding. - NO RESTRICTION in Code

 

Condition 2

I use a Flux from manufacturer ABC and wire from manufacturer XYZ. Manufacturer ABC who is the manufacturer of Flux has certified the flux on bag as F7A8-EH12K (when I say this, I mean the manufacturer ABC has used both flux and wire from manufacturer ABC)

 

My actual conditions are I am using different manufactures for flux and wire to qualify PQR

PQR was qualified with PWHT

Question

1.       Can I use different manufacturer for flux and wire - NO Code restrictions unless specifically restricted in the Specification

2.       Can I write on my PQR and WPS write the Flux wire classification as F7P8-EH12K - NO

3.       Batch of flux and wire used in PQR shall only be used in Production welding. _ NO

 

Appreciate your advice for me to understand and if any reference document which I can review of the subject to clarify.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/0f907ff4-734e-4084-8059-127bb4b37b5dn%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...