Dear Experts,

I am following up on my earlier emails regarding the alignment of weld seams on SS304 pipes and their reinforcing pads (RF pad). I have not yet received a response and would greatly appreciate your expert opinion on the matter.

To recap: Is aligning the EFW seam of the pipe with the manually welded seam of the RF pad in the same straight line acceptable per ASME standards?

Are there any minimum distance requirements between the pipe seam and the RF pad weld joint, as per the relevant ASME code sections?

Your prompt guidance would be greatly appreciated to ensure compliance with the necessary standards.

Thank you again for your time, and I look forward to your response.


Best regards,
Vinoth G


On Thu, 27 Mar 2025 at 20:23, Vinoth Kanna <gvinoth43@gmail.com> wrote:
Dear Experts,

I would like to seek clarification regarding the alignment of the weld seams on SS304 pipes and their reinforcing pads (RF pad). Referring to the attached photo, the EFW seam of the pipe and the manually welded seam of the RF pad are aligned in the same straight line.

Could you please confirm whether this is acceptable as per ASME standards? Also I would appreciate it if you could specify the relevant ASME code section and highlight if there is any minimum distance requirement between the pipe seam and the RF pad weld joint.

Your expert guidance on this matter will be highly valuable.


Best regards,

Vinoth G

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BoUWirva1vFd87uHFquQO%2BO_2wSubqTWyg2q2hcwoXTu-sNTQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...