Re: [MW:35512] ASME SEC IX JOJNT DESIGN

Dear Mr. Elavarasan,
As per ASME Section IX, a Welding Procedure Specification (WPS) does not strictly require a joint design 
sketch, but it must address certain variables such as groove design and root spacing. These variables are 
considered non-essential for most welding processes, meaning changes in them do not require requalification 
of the procedure. However, they must be specified in the WPS to guide the welder.
1.Groove Design: While a change in groove design is a non-essential variable for most processes, the WPS should 
   specify the types of joints permitted in production. Stating "all groove designs" is not acceptable; instead, the WPS 
   should list specific types (e.g., V-groove, U-groove) or reference a drawing that illustrates the allowable joints.
2. Root Spacing: This is also a non-essential variable. The WPS should address root spacing but does not need to 
    include a sketch. However, if a sketch or drawing is used, it must be accessible to the welder and accurately depict 
    the joint details.

Client's Request:
Your client's request to add a sketch (like root gap, root face, included angle) to the WPS is reasonable for clarity and 

to ensure that the welder understands the joint requirements. While not mandatory, including such details can enhance 

the WPS's effectiveness in guiding the welder and ensuring consistency in production welds.

Best Practice:

  • Include specific details about the joint design in the WPS.

  • If a sketch is added, ensure it is clear and accessible to the welder.

  • Alternatively, reference a manufacturing drawing that includes these .

Trust it is clear,
rgds,
C Sridhar.

On Sun, 6 Apr 2025 at 08:45, Elavarasan Mech <elavarasan1861994@gmail.com> wrote:

Dear expert 

As per ASME SEC IX in WPS  joints design sketch is required or not  .our client commented in our WPS need to add sketch (like root gap, root face ,included angel )please guide me 


Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4y%3DSdC%2BViuR1doMm4xBi6t%2BKi-3agpW%2BHv-mAOHXB1fMfQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYijfWiYza2FnSciua3w_vdWvVL2hhEbP1yFnhPjrHnzH1Q%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...