Re: [MW:33783] Filler wire Button weld test

Hi
There are NO code requirements for button weld test. Kindly review project specification or ask the client the reason for the button weld test. Maybe he has a doubt about the electrode or something like this.

Regards 

On Tue, Nov 29, 2022 at 1:05 PM Faisal Quadri <faisalquadri12@gmail.com> wrote:
SAES A 206  Aramco requirement 

On Tue, Nov 29, 2022, 1:25 PM Ponnikumar <k.ponni1994@gmail.com> wrote:
Dear gentlemen,
My client inspector told me to do button weld test on plate for filler wire 309L . The dimension are follow as asme sec II c then need to do PMI verification 

My query is any requirements by code for filler wire button test for all filler and electrode and why it required ? 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYw73OyFYLq4yTHUB2cVqbuaDCCunxc73%2BaU0kJZurJd%2Bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJwxg4e8MUi3dCWRoVTdphw1FNueJuUc8WcucN1nUtd58emFZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVihPmRR9dHUR_KX5MLrYj0PnB6s7qm%2BKaguD7ooEpk60TvQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...