Re: [MW:33768] FILLER WIRE FOR SS 304 TO SS321

why don't use 321 when TIG is engaged 

On Fri, Nov 25, 2022, 8:45 AM M.Sathiya Narayanan <gmvsathya@gmail.com> wrote:
use 347 composition 

On Wed, Nov 23, 2022 at 2:48 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear experts

what will be the filler wire for SS304 TO SS321 MATERIAL






Best Regards
Sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMw1hbRkNUXRkD%3DW4wosZ02_Mr1-0HBvqii3%2Bh1-DBa4A%40mail.gmail.com.


--
Thanks and Regards
M.Sathyanarayanan
0091-7358752505

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzo-ktUPmQmWNe27BG8k6O0XwzfjhZzepuHdXfh1H%2BtiMJJCQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOScREskxbZp%3DcvybYq7FbQzMLGzRx1Fb%2BWotww-vCTTQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...