Re: [MW:33756] SS PIPE ASTM 554 TYPE 304

Dear Expert.
Thank you for your information, 

If we will use 316L filler wire what is the effect for welding?



On Mon, Nov 21, 2022 at 9:56 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
308
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Nov 12, 2022 at 6:38 PM Simhachalam Battini <simhachalam.battini729@gmail.com> wrote:
Dear All,

Great to hear from you.

Which filler is required to weld ss Pipe to Pipe  ASTM A554 Type 304.


Thanks, Regards.

 

Battini Simhachalam

QC Inspector – Quality Dept. 

ArRiyadh New Mobility - CWG

6th Floor, ArRiyadh New Mobility Building

Olaya Street (North) – Al Sahafah District

P.O. Box 99816 – Riyadh 11625 – Saudi Arabia

M +966 546044327

simhachalam.battini@cwg-metro.com

www.anm-metro.com

24°46'57.42"N  46°38'26.10"E

Location map (click here)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABk4cbF476CBNYD5%2By1NJAYOZVXZKFNWe0tuiV%2B1SV%2BipuhwMw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMmYQPpj3B9gcbVG6QQ8sfiKH3y7L4hRxLzZWUEDi67gg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABk4cbEbx2x%2BXXcRV8rawGyXhUAWwvGfajsLoBpoUjx_RWpF%2Bw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...