Dear Sir,
Greetings!!

Thanks for your email.
In our case we are using the Neutral Flux Combination.
Data sheet is attached below FYR

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message


On Mon, Nov 14, 2022 at 12:42 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
is it active flux, if so u will have more Mn^Si which are added through flux while welding

On Mon, Nov 14, 2022, 8:50 AM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,

As per Sec.IX. Table QW-442 (A Numbers) for A-No.1, Mn (Max %) is 1.60 , but one of our Kiswel SAW MTC is having 1.63 (wt. %) Mn in the chemical composition of the weld metal under PWHT Condition (602 Deg.C x 9 Hrs) - It can be considered under A No.1 - Please confirm

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ40m1NOWXEgi-%2BYWy7wzAe1UY7ND%3DhiegCtsf6%3DDc2DMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMCJntGJ4N%2Bfgw_0Q1ksEm3aa8JR6%2BBirC62p%3DD5UrASQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ4GBLa77D7-RkFoXTGb9T2tzWFLxdcmUGV4paD5fGRF2A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...