Mr. Vishal, E6010 not require any backing or heating due to cellulosic flux.

Best Regards,

cid:image001.png@01D0FB95.19500D80

Muhammad Babur Khan Lashari
Mechanical Inspector ( Piping / Welding)

Inspection Department
Mob: +966 58 2774568 / 55 968 0573

          +92 334 6186285

Applus Velosi Saudi Arabia

Please consider the environment before printing this e-mail



On Tue, Nov 15, 2022 at 8:26 AM Vishal Jaiswal <vis469jaiswal70@gmail.com> wrote:
Dear Sir,

               Please give information about ER 6010 electrode is need baking or holding in portable oven for the root welding of ERW pipes having thickness range 3 to 8 mm.
Please give suggestions.



Thanks and regards
Vishal kumar
Mechanical Engg.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t408Ks6qVdKS5qRuS06scPKDDzchmwsx01G20H3kb7Z71Tg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN53wK2sF41YELtXb0ud81ZZ6dvv4Ak5d05dja_fjgeunWqWMA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...