Wednesday, November 9, 2022

Re: [MW:33673] Regarding Flush Grind of weld Reinforcement

IBR, 
and others also.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Nov 9, 2022 at 9:50 AM Manoj Singh <manoj.singh1178@gmail.com> wrote:
Thanks for your kind reply sir, is there any standard requirement, refers in this case pls let me know.

On Wed, 9 Nov 2022 at 9:08 AM, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
it can be flush ground because while doing PQR, we are testing without reinforcement. Since it is difficult to weld flush with base metal that is why some reinforcement based thickness is allowed. If u want to  take RT keep some reinforcement for density difference.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Nov 9, 2022 at 8:54 AM Manoj Singh <manoj.singh1178@gmail.com> wrote:
Hi All,

Can anyone please provide the details regarding the said subject, whether it is allowed and if yes what are the criteria to be followed in the terms of NDT,
along with the  standards codes if any.

Thanks in advance.

With regards,

Manoj Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRJwQwOUFjfwEFvOrzF1g0bmodAswCFVrS-JstH%3DTOvX4w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmeRR93kUbpqH_%3DbvofF7WiB%2BwU1a%2BmfLQyOEmr70F%2Bg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdR%2BTt%3DrTnUjZ6pPXSZSynLJ%2B%2BTgjo9e88_6yWzXFZ-wjRQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMwvL4yJse5Rw4ZEyM5tyEV%3DvzDXMcDoPAu-jyxjx7uxg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...