Hi
By mistake or not protecting (no masking tape) the serrated surface, the painting contractor might be painted, surface preparation and painting is not allowed on serrated surfaces.
During transportation after manufacturing, the serrated surfaces should be applied with corrosion protective coatings for preservation until usage.
Regards
Govindan Perumal
On Mon, Nov 7, 2022, 08:12 madhan chozhan <madhanchozhan@gmail.com> wrote:
Good day Gents,--I would like to understand from the experts on the below.1. Is painting on the flange serrations for both RF and FF flanges allowed. If yes which code/specifications mandates it and if no which code/specifications mandates it.2. Is there a way to do preparation for painting on the serrations without damaging the serrations.Best Regards,Madhan
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABnNWHW9aKSTSk%2BX%3DKAT4DqfRErG_5nyJhbocHX9-jRFux7Xeg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fy1bJWBqmbwxbBtWzX7RU_8nUjFEgD4cxN_vgL-8o3EQ%40mail.gmail.com.
Comments