[MW:33723] Re: Need your support to prepare WPS , PQR & WQTR - Alloy 625 + Sttellite

Dear Experts, 

Please need your audience to prepare WPS, PQR, & WQTR.
Please refer to my query and update me.

On Monday, November 14, 2022 at 2:55:44 PM UTC+5:30 Kiran Ekbote wrote:
Dear All,

Please support me to prepare  WPS, PQR & WQTR.
Details as below - 

Base Material – ASTM A 494 Gr. CU5MCUC.

Location to weld – Seat ring Area (Valve Seat ring).

Alloy 625 + Sttellite.

Base materials thickness – 15 mm

Welding Process - PTA Process (Plasma transferred arc welding).

Please let me know for P No, A No, F No. welding rod, and let me know any guidance on  ASTM A 494 Gr. CU5MCUC qualification and requirements and sample WPS and PQR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7f6d5604-ce08-45e2-bde8-8390b2ff4769n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...