Friday, November 11, 2022

[MW:33680] Re: Heat input calculation for Pulsed GTAW process

(1) for instantaneous energy measurements in
joules (J) Heat input [J/in. (J/mm)]
409.1.png

regards,
siraj.

On Friday, November 11, 2022 at 6:21:32 AM UTC+3 manivannan hemu wrote:
Dear Experts,

Please provide Heat input calculation-formula for Pulsed GTAW welding process with reference to code/standards.

Thanks,

MANIVANNAN.P

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0828fc04-1938-40a0-9cf0-04c44423da8an%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...