[MW:33655] E 7018 or E 7018-1

Dear Experts,
Greetings to all.

Could you please suggest suitable SMAW welding electrode (E 7018 or E 7018-1) for the below specifications,

MOC                                                   : SA 516 Gr.70 + N , 70 mm Thickness
PWHT                                                 :  610 ° C x 300 minutes minimum
Impact Test after HT                             :  -29° C
Weld Metal & HAZ Hardness (Max.) : 22 HRC

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ54pJFzsM7_C_vd8EQ80eXy86A9CP38Kbh3%2BKKNHaJKyQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...