Re: [MW:31062] What is the technical explanation of : "weaving shall be three times of electrode core diameter"

Dear SIr
Do As much as the Weaving  wish to do during  establishment of PQR  report the same on the witness sheet. Once the test reports  are Ok. Mention the weaving range on WPS ( Such as max. Weaving allowed 20 mm.). I do the same thing and don't face any issues from customers as well as TPI  Because It is tested and reported on PQR .
Regards
Atul Jha 

On Sun, Jun 28, 2020 at 9:48 PM Aakash <harenathjha@gmail.com> wrote:
Hello Experts,
What is the technical explanation of : "weaving shall be three times of electrode core diameter"
or any code reference ?

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c10f8b8-5359-4c59-907e-de6c9c3f43ado%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC1tTULAEQxscDR1dUi5CayiBqGtDXUp9X1fao9Y-A3jGeRN8A%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...