Monday, June 29, 2020

Re: [MW:31062] Impact Sub-size specimen

Hi

Temperature reduction is applicable for sub size specimen and there is no relaxation for joule value.

Sent from my iPhone

> On 28-Jun-2020, at 11:44 AM, ABHISHEK SINGH <mech.abhi17@gmail.com> wrote:
>
> Dear Experts,
>
> I am having query regarding impact test as per ISO EN standard.
> 1) Is any temperature reduction is applicable for impact sub-size specimen?
> 2) Any joule value relaxation for impact sub-size specimen.
>
> Regards
> Abhishek Singh
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c9483c40-6376-464d-8a60-e49476993fc7o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B3C65D9D-BCE1-449E-A808-509263876D4B%40gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...